The GATE Grind

GATE Engineering Materials: Phase diagrams and heat treatment – Previous Year Questions

13 GATE previous year questions on Phase diagrams and heat treatment (Engineering Materials, Mechanical Engineering) with answers and explanations, from every paper.

13 questions worth 17 marks in all (9 1-mark, 4 2-mark). Asked between 2016 and 2025, so you can see how the topic has been tested over time.

  1. GATE 2016 ME (ME2) Q31 (1 mark, Multiple choice) – In the phase diagram shown in the figure, four samples of the same composition are heated to temperatures marked by a, b, c and d. At which…
  2. GATE 2016 ME (ME2) Q58 (2 marks, Multiple choice) – In a binary A–B system, liquid containing 20% A coexists with solid containing 70% A. At overall composition 40% A, the solid fraction is .
  3. GATE 2016 ME (ME1) Q30 (1 mark, Multiple choice) – The “Jominy test” is used to find
  4. GATE 2018 ME (ME2) Q22 (1 mark, Multiple choice) – L denotes liquid and M solid; subscripts distinguish phases. A eutectoid reaction is .
  5. GATE 2019 ME (ME2) Q24 (1 mark, Multiple choice) – Hardenability of steel measures .
  6. GATE 2019 ME (ME2) Q44 (2 marks, Multiple choice) – The binary phase diagram of P and Q is shown. Alloy X contains 60 wt% P and 40 wt% Q and cools from liquid to solid. Find solid and liquid weight…
  7. GATE 2020 ME (ME2) Q21 (1 mark, Multiple choice) – Which statement about a phase diagram is INCORRECT?
  8. GATE 2020 ME (ME1) Q21 (1 mark, Multiple choice) – Match each heat treatment with its effect. P: Tempering; Q: Quenching; R: Annealing; S: Normalizing. Effects: 1: Strengthening; 2: Toughening; 3:…
  9. GATE 2021 ME (ME2) Q14 (1 mark, Multiple choice) – The Cast Iron which possesses all the carbon in the combined form as cementite is known as
  10. GATE 2022 ME (ME1) Q41 (2 marks, Multiple choice) – In Fe-Fe 3C phase diagram, the eutectoid composition is 0.8 weight % of carbon at 725 °C. The maximum solubility of carbon in α-ferrite phase is 0.025…
  11. GATE 2023 ME Q52 (2 marks, Numerical answer) – A steel sample with 1.5 wt.% carbon (no other alloying elements present) is slowly cooled from 1100 °C to just below the eutectoid temperature (723…
  12. GATE 2024 ME Q28 (1 mark, Multiple choice) – The phases present in pearlite are
  13. GATE 2025 ME Q20 (1 mark, Multiple choice) – Among the following surface hardening processes, steel is heated to the lowest temperature in