GATE 2023 XE — all source sections – Question 60
A pure Silicon wafer is doped with Boron by exposing it to B2O3 vapour at an elevated temperature. It takes 1000 seconds to reach a Boron concentration of 1020 𝑎𝑡𝑜𝑚𝑠 𝑚 − 3 at a depth of 1 µm. The time taken to reach the same concentration of Boron at a depth of 2 µm is (in seconds): _________ (rounded off to nearest integer) Given: Boron concentration on the wafer surface remains constant.
Practise this question in The GATE Grind →
Show answer and explanation
Correct answer: 3840 to 4100
Explanation
With constant surface concentration and diffusivity, the semi-infinite diffusion profile depends on x/√t. Reaching the same concentration at twice the depth therefore needs four times the duration. The time is 4 × 1000 = 4000 s. Surface and initial concentrations cancel from this same-profile comparison.