GATE 2024 XE — all source sections – Question 66
The engineering stress (𝜎) vs. engineering strain (𝜀) curve obtained by conducting uniaxial tension test on a steel specimen is shown in the figure (the sketched curve is not to the scale). The specimen exhibits cup-and-cone failure within its gage length. Which point on the curve corresponds to the beginning of necking in the test specimen?

Practise this question in The GATE Grind →
Show answer and explanation
Correct answer: (D) S
Explanation
Necking begins at the maximum engineering stress, where the tensile force reaches its peak before localized area reduction dominates. That point is S, D. P, Q mark the yield region, and R the end of the yield plateau rather than the start of necking.