27 questions worth 41 marks in all (13 1-mark, 14 2-mark). Asked between 2016 and 2026, so you can see how the topic has been tested over time.

  1. GATE 2017 ME (ME1) Q31 (1 mark, Numerical answer) – A material has just begun yielding in metal forming, with principal stresses 1=180 MPa, 2=-100 MPa, 3=0. By von Mises theory, find its uniaxial yield…
  2. GATE 2016 ME (ME3) Q31 (1 mark, Multiple choice) – Equal amounts of a liquid metal at the same temperature are poured into three moulds made of steel, copper and aluminum. The shape of the cavity is a…
  3. GATE 2016 ME (ME2) Q59 (2 marks, Numerical answer) – Gray cast iron blocks of size 100 mm × 50 mm × 10 mm with a central spherical cavity of diameter 4 mm are sand cast. The pattern shrinkage allowance…
  4. GATE 2016 ME (ME1) Q32 (1 mark, Multiple choice) – The part of a gating system which regulates the rate of pouring of molten metal is
  5. GATE 2016 ME (ME1) Q59 (2 marks, Numerical answer) – Heat is removed from 2 kg of molten metal at a constant 10 kW until complete solidification. The cooling curve is shown. Assuming uniform temperature…
  6. GATE 2016 ME (ME1) Q61 (2 marks, Multiple choice) – A cylindrical job with diameter of 200 mm and height of 100 mm is to be cast using modulus method of riser design. Assume that the bottom surface of…
  7. GATE 2017 ME (ME2) Q35 (1 mark, Multiple choice) – A T-shaped cross section is to be made from a rectangular aluminium block. Which process is expected to give the highest strength?
  8. GATE 2017 ME (ME2) Q60 (2 marks, Multiple choice) – A 20 mm rod is stretched to 40 mm, then compressed to 10 mm. With tensile longitudinal strain positive and compressive strain negative, its total true…
  9. GATE 2017 ME (ME2) Q62 (2 marks, Numerical answer) – A 120 mm wide, 8 mm thick strip passes between two 300 mm diameter rolls to become 7.2 mm thick, retaining its width. Exit speed is 30 m/min. With no…
  10. GATE 2018 ME (ME2) Q23 (1 mark, Multiple choice) – During solidification of a pure metal, the casting grains near the mould wall are .
  11. GATE 2018 ME (ME2) Q60 (2 marks, Numerical answer) – A solid cylindrical riser with height equal to diameter is required for sand casting an 80 mm × 120 mm × 20 mm rectangular plate. Casting…
  12. GATE 2019 ME (ME2) Q25 (1 mark, Multiple choice) – Fluidity of molten cast alloys, without flux addition, increases with increased .
  13. GATE 2019 ME (ME2) Q60 (2 marks, Numerical answer) – The shown metal-block pouring arrangement has negligible friction. With g = 9.81 m/s², find time to fill the 40 cm × 30 cm × 15 cm mould cavity (s),…
  14. GATE 2019 ME (ME1) Q23 (1 mark, Multiple choice) – In casting, the vertical passage carrying molten metal downward from pouring basin to runner is called .
  15. GATE 2019 ME (ME1) Q47 (2 marks, Multiple choice) – Match casting defects P: blow hole, Q: misrun, R: hot tearing, S: wash with causes 1: poor collapsibility, 2: mould erosion, 3: poor permeability, 4:…
  16. GATE 2020 ME (ME2) Q52 (2 marks, Numerical answer) – A 1200 cm³ mould cavity fills through a 10 cm long sprue feeding a horizontal runner. Sprue base area is 2 cm². For g = 9.81 m/s² and negligible…
  17. GATE 2021 ME (ME2) Q47 (2 marks, Numerical answer) – A cast product of a particular material has dimensions 75 mm × 125 mm × 20 mm. The total solidification time for the cast product is found to be 2.0…
  18. GATE 2021 ME (ME1) Q46 (2 marks, Numerical answer) – A true centrifugal casting operation needs to be performed horizontally to make copper tube sections with outer diameter of 250 mm and inner diameter…
  19. GATE 2022 ME (ME2) Q19 (1 mark, Multiple choice) – Fluidity of a molten alloy during sand casting depends on its solidification range. The phase diagram of a hypothetical binary alloy of components A…
  20. GATE 2022 ME (ME2) Q27 (1 mark, Multiple select) – Consider sand casting of a cube of edge length a. A cylindrical riser is placed at the top of the casting. Assume solidification time t s V/A, where V…
  21. GATE 2023 ME Q25 (1 mark, Multiple select) – In a metal casting process to manufacture parts, both patterns and moulds provide shape by dictating where the material should or should not go. Which…
  22. GATE 2024 ME Q31 (1 mark, Multiple choice) – The allowance provided to a pattern for easy withdrawal from a sand mold is
  23. GATE 2024 ME Q61 (2 marks, Numerical answer) – Aluminium is casted in a cube-shaped mold having dimensions as 20 mm × 20 mm × 20 mm. Another mold of the same mold material is used to cast a sphere…
  24. GATE 2025 ME Q34 (1 mark, Numerical answer) – A liquid metal is poured in a mold cavity of size 200 mm 200 mm 200 mm. The cooling is uniform in all directions with NO additional compensation for…
  25. GATE 2025 ME Q38 (2 marks, Multiple choice) – Match the mold elements in the casting process with the most suitable function Mold element Function --- --- --- --- P Blind riser I Casting with…
  26. GATE 2025 ME Q62 (2 marks, Numerical answer) – Two metal parts (a cylinder and a cube) of same volume are cast under identical conditions. The diameter of the cylinder is equal to its height. The…
  27. GATE 2026 ME Q30 (1 mark, Multiple choice) – In relation to metal casting defects, match the following Defect Description --- --- --- --- P Dross I Shallow blow found on a flat casting surface Q…