GATE Casting, Forming and Joining Processes: Welding, brazing, soldering and adhesive bonding – Previous Year Questions
19 GATE previous year questions on Welding, brazing, soldering and adhesive bonding (Casting, Forming and Joining Processes, Mechanical Engineering) with answers and explanations, from every paper.
19 questions worth 28 marks in all (10 1-mark, 9 2-mark). Asked between 2016 and 2025, so you can see how the topic has been tested over time.
- GATE 2017 ME (ME1) Q33 – In arc welding, travel speed is doubled while all other process parameters remain constant. The weld-bead cross-sectional area will
- GATE 2016 ME (ME3) Q58 – Two 2 mm steel sheets are spot welded with 4 kA for 0.2 s. The cylindrical weld nugget diameter is 5 mm. Steel latent heat of fusion is 1400 kJ/kg,…
- GATE 2016 ME (ME2) Q32 – The welding process which uses a blanket of fusible granular flux is
- GATE 2016 ME (ME2) Q60 – In DC arc welding, V=100+40l, with arc length l in mm and voltage V in volts. During welding, l varies from 1 to 2 mm and current ranges from 200 to…
- GATE 2016 ME (ME1) Q31 – Under optimal conditions of the process the temperatures experienced by a copper work piece in fusion welding, brazing and soldering are such that
- GATE 2018 ME (ME2) Q63 – A welding operation uses 30 V and 100 A. Weld-bead cross-sectional area is 20 mm². Workpiece and filler are titanium with specific melting energy 14…
- GATE 2018 ME (ME1) Q22 – The shaded weld shown is a weld.
- GATE 2019 ME (ME2) Q61 – Gas tungsten arc welding uses 250 A, 20 V and travel speed 5 mm/s. Arc efficiency is 70%. Find net heat input per weld length (kJ/mm), to one decimal…
- GATE 2019 ME (ME1) Q24 – Which welding method gives the highest heat flux (W/mm²)?
- GATE 2020 ME (ME2) Q20 – Two 6 mm thick plates are butt-welded. Select the processes in INCREASING order of heat-affected-zone size: 1: Arc welding; 2: MIG welding; 3: Laser…
- GATE 2021 ME (ME2) Q48 – A spot welding operation performed on two pieces of steel yielded a nugget with a diameter of 5 mm and a thickness of 1 mm. The welding time was 0.1…
- GATE 2021 ME (ME1) Q47 – The resistance spot welding of two 1.55 mm thick metal sheets is performed using welding current of 10000 A for 0.25 s. The contact resistance at the…
- GATE 2022 ME (ME2) Q57 – In a direct current arc welding process, the power source has an open circuit voltage of 100 V and short circuit current of 1000 A. Assume a linear…
- GATE 2022 ME (ME1) Q57 – Two mild steel plates of similar thickness, in butt-joint configuration, are welded by gas tungsten arc welding process using the following welding…
- GATE 2023 ME Q23 – Two surfaces P and Q are to be joined together. In which of the given joining operation(s), there is no melting of the two surfaces P and Q for…
- GATE 2024 ME Q32 – The most suitable electrode material used for joining low alloy steels using Gas Metal Arc Welding (GMAW) process is
- GATE 2024 ME Q63 – In an arc welding process, the voltage and current are 30 V and 200 A, respectively. The cross-sectional area of the joint is 20 mm2 and the welding…
- GATE 2025 ME Q21 – The welding process commonly used for fabricating tailor-welded blanks of dissimilar thickness for automotive applications is
- GATE 2025 ME Q33 – During a welding operation, thermal power of 2500 W is incident normally on a metallic surface. As shown in the figure below (figure is NOT to scale),…